These Several Reasons Will Cause the Jaw Crusher Frame to Break

Apr 10, 2025

Leave a message

1.Low ambient temperature
Since the welding was carried out in winter, the ring - tightening temperature was lower than 0 °C. When welding at low temperature, the weld metal cooling rate is faster, and the tendency to crack becomes greater. In particular, for Q345, since its alloying element content is higher than that of low - carbon steel, its hardening tendency is greater than that of low - carbon steel, and the tendency to crack during low - temperature welding is even greater.
2. Crusher welding rod drying

When welding the jaw crusher frame, the welding seams are formed by manual arc welding, and the welding rod used is the low - hydrogen type E5016. Before welding, the electrode is required to be dried at 350 - 400 °C for 2 hours, and after heat preservation, it can be used as required. However, by tracking the welding process, it is found that the drying temperature of the electrode is only about 200 °C, so that the moisture adsorbed in the electrode coating and the crystalline water in the coating composition cannot be removed, and the likelihood of gas formation and cracking caused by water increases.

 

news-1000-496

 

3. Weldment cleaning

Since the E5016 welding rod is sensitive to water, oxides, rust, and oil on the weldment surface, the surface of the weldment needs to be strictly cleaned to prevent porosity. However, the actual cleaning process during welding is not strict, so the likelihood of porosity and cracking increases.

Send Inquiry
Contact usif having any question

You can contact us via phone, email, or the online form below.Our specialist will contact you shortly.

Contact now!